Hastelloy:
This material is universally used in valves and pumps where the greatest resistance is required to corrosion caused by strongly oxidising acids.
Hastelloy-C276 is resistant to strongly oxidising agents such as chlorine, nitric, acetic, formic, phosphoric, sulphuric and hydrofluoric acids, zinc chloride and ammonium solutions, water-based solutions containing chlorine or hypochlorites and acid solutions of ferric and cupric salts.
Hastelloy-D is exceptionally resistant to any concentration of sulphuric acid, up to its boiling point.
Cu | Tungsten | Mo | Fe | Cobalt | Ni | Grade | Hardness | |
Hastelloy C 276 | 14.5-16.5% | 3-4.5% | 15-17% | 4-7% | 2.5% max. | Balance | 100, 200 | 170-185 Hv |
Hastelloy B2 | 1.00 max. | 3-4.5% | 26-30% | 2 max | 1.00% max. | Balance | 100, 200 | 170-185 Hv |
Hastelloy D | 1.00 max. | 3-4.5% | 15-17% | 2 max | 1.50% max. | Balance | 100, 200 | 170-185 Hv |